Galvanic Corrosion

Galvanic Corrosion Defined: When two different metals are immersed in a corrosive solution, each will develop a corrosion potential. If the corrosion potential of the two metals is significantly different, and they are in direct contact and immersed in an electrolyte, the more noble metal will become the cathode and the more active metal will become the anode. A measurable current may flow between the anode and the cathode. The corrosion rate of the anode will be increased and the cathode decreased. The increased corrosion of the anode is called "galvanic corrosion". In the presence of an electrolyte such as moisture (especially salt water) the two metals are "bridged", forming an electrical couple.  Once the couple is created there is an exchange of electrons.  In layman's terms, one metal extracts mass from the other, thus causing corrosion.  If you have ever seen a white chalky substance on thresholds you have seen galvanic corrosion. 

Requirements for Galvanic Corrosion: In order for galvanic corrosion to occur, three elements are required. If any of these elements is missing, galvanic corrosion cannot occur. If, for example, the direct contact between the two metals is prevented (plastic washer, paint film etc.) there cannot be galvanic corrosion.

1)   Dissimilar metals
2) Metal-to-metal contact
3) Metals in the same conduction solution (usually called an electrolyte)\

The greater the corrosion potential of each metal (the more active or more noble) the greater the potential for corrosion. The "galvanic series" has been developed to list the various metals in order from most active to most noble:

Magnesium

Anodic

Galvanized Steel

 

Aluminum

Mild Steel

Low Alloy Steel

Cast Iron

Lead

Tin

Muntz Metal

Yellow Brass

Red Brass

Copper

Aluminum Bronze

Silver

Stainless Steel (430)

Stainless Steel (304)

Stainless Steel (316)

Monel

Silver

Titanium

Gold

Cathodic

The greater the separation between the two metals listed, the greater the corrosion potential. For example, if zinc (think galvanized steel) which is an active material and near the top of the list and stainless steel, a noble metal and near the bottom of the list were in direct contact and in the presence of an electrolyte (water), galvanic corrosion will probably occur.

In addition to the three elements sighted above, the relative area of each of the exposed metal surfaces is also a consideration (see Figure below). If the area of the cathode (noble metal) is very large, and the anode (active metal) is very small, the current produced is likely to be very high and the anode will corrode quickly. For example, if there is a window frame made of stainless steel and it is attached with carbon steel screws, the screws will probably corrode. If the area of the cathode (noble metal) is very small, and the anode (active metal) is very large, the current produced will be very low and the anode will corrode very slowly, if at all. If the window frame is made of carbon steel and it is attached with stainless steel screws there will be very little, if any, corrosion.

Dissimilar metal combinations should be avoided in areas where moisture is likely to accumulate and remain for long periods. In well drained exterior applications, dissimilar metals can be used together if favorable surface ratios exist, but the best solution is to electrically insulate one from the other. When painted carbon steel and stainless steel are welded together, the welded joint should be painted. Stainless steel fasteners with neoprene or other inert washers are regularly used with other metals.